Product Details
Place of Origin: GuangZhou, China
Brand Name: RUI - HE
Certification: RoHS, FDA, MSDS, SGS, REACH, PAHS, ISO9001:2016, etc.
Model Number: RH5011F
Payment & Shipping Terms
Minimum Order Quantity: 20KG or 2000KG
Price: Negotiation
Packaging Details: 20 kg pails or 200 kg drums
Delivery Time: 5 -15 days
Payment Terms: Western Union, L/C, T/T, Paypal
Supply Ability: 1000 tons per day
Port: |
GUANGZHOU / SHENZHEN |
Service: |
ODM / OEM |
Curing Type: |
DBPH |
Sample: |
Available |
Name: |
100% Silica |
Selflife: |
3 Years |
Color: |
Semi-transparent |
Work Process: |
Compression Machine |
Port: |
GUANGZHOU / SHENZHEN |
Service: |
ODM / OEM |
Curing Type: |
DBPH |
Sample: |
Available |
Name: |
100% Silica |
Selflife: |
3 Years |
Color: |
Semi-transparent |
Work Process: |
Compression Machine |
Description
This RH5011F is a kind of pourable, addition-curing, two-component silicone rubber that vulcanizes at low temperature. RH7011 is non-toxic and good transparency liquid silicone rubber.
Typical Properties
RH5011F |
|||
Properties |
Unit |
|
|
Appearance |
/ |
translucent |
|
Density |
g/cm3 |
1.22 ± 0.02 |
|
Shore A Hardness |
A/JLS |
52 |
|
Tensile Strength |
MPa |
≥ 9.0 |
|
Elongation at break |
% |
≥ 450 |
|
Tear Strength |
KN/m |
≥ 18 |
|
Linear Shrinkage |
% |
≤ 0.1 |
|
Tensile set |
% |
≥ 9 |
|
Rebound |
% |
≥ 50 |
|
Plasticity |
% |
250-310 |
These figures are for reference only, please contact us for details.
Why do you choose RH5011F
Good transparency
High stability to ozone
UV light resistance
Micro-crack resistance
High transparence / Good transparency
High tear and tensile strength
Good rebound property
Excellent resistance to acid and alkali
Neutral odor and taste
Sterilizable with ethylene oxide, steam and gamma radiation
Certificate
Rui-He RH5011F® silicone rubber obtained the following test certificate: RoHS, FDA, REACH, PAHS, ISO9001:2015, etc.
Packaging & Storage
Available in 20kg cartons.
Store in a cool, dry place out of direct sunlight, use it within 12 months from the day of manufacture.
FAQ
Q: Why is the tear strength of the silicone mold weak?
A: There are three reasons:
In order to reduce the viscosity of silicone rubber and pursue a good quality, you may add a lot of silicone oil into the silicon rubber when making molds. In fact, it might have just the opposite effect. The tension and the tear strength will be reduced badly with the addition of silicon oil. And the silicon molds will be in a weak and flimsy manner.
You may add too much catalyst into the silicone rubber, we suggest customers add catalyst no more than 5%, 2%will be perfect.
You may use the silicone mold too early after it finished. We suggest the customer begin using the molds after 24 hours. What’s more, it will be better if you can make an outer mold to protect the silicone mold.
Notice
This product cannot be contacted with compounds containing N, P, S to avoid affecting the catalytic effect of platinum.
If you need to know the prices of our silicone rubbers, please contact us. We do not provide prices on the website because prices fluctuate for many reasons.